A turbine developer needed prototype impellers in 7075-T6 aluminum for wind-tunnel testing, with blade walls of 0.8 mm and a surface finish that would not disturb airflow.
Project Background
Each impeller had 17 blades with variable twist, a 0.8 mm nominal wall, and a hub bore held to ±0.01 mm. Surface finish on the blade surfaces had to reach Ra 0.4 μm, and the program required 20 parts across four design revisions.
The Engineering Challenge
Blade deflection during machining caused wall thickness to vary by more than 0.15 mm, and the first two revisions were scrapped at an 18% rate. Chatter on the thin trailing edges also produced visible marks that required manual polishing, which risked changing the airfoil profile.
We re-sequenced the toolpath from hub to tip, reduced radial engagement, and added a sacrificial wax support on the trailing edges. A 5-axis finishing pass at constant chip load replaced the previous 3-axis approach, and blade thickness was measured on a CMM after each part.
Impact and Results
Wall thickness held within ±0.03 mm, Ra 0.4 μm was achieved directly off the machine with no manual polishing, and scrap dropped from 18% to 3%. Machining time per impeller fell 22%, which allowed all four design revisions to be tested within the original schedule.